SR EN ISO 787-9:2003
Metode generale de încercare pentru pigmenţi şi materiale de umplutură. Partea 9: Determinarea pH-ului unei suspensii apoase
The water used shall be freshly distilled water, boiled before use, but for 5 to 10 min only, in order to avoid an increase of its pH value due to alkali dissolved from the glass. Preparation of a suspension of the material under test, stopper the container, shaking, allow to stand any time, removing the stopper and determination, to the nearest 0.1 unit, of the pH value of the suspension. - Cancels and replaces ISO Recommendation R 787/9-1970.
Status :
Anulat
Data aprobării : 21.04.2003
Data publicării : 22.04.2003
Data anulării : 30.08.2019
Număr de pagini : 10
ICS : 87.060.10 Pigmenti si materiale de umplutura
Comitet tehnic : 338 - Lacuri, vopsele, cerneluri, răşini, pigmenţi anorganici şi adezivi
- Inlocuieste SR ISO 787-9:1995
- Inlocuieste STAS 7948/8-69
- Inlocuit prin SR EN ISO 787-9:2019
- A99 SR ISO 787-9:1995/A99:2003
EN